如何解決防火板加工時出現(xiàn)的爆邊問題?
來源:http:/// 日期:2021-05-07 發(fā)布人:admin
如何解決防火板加工時出現(xiàn)的爆邊問題?
How to solve the problem of edge burst in the processing of fireproof board?
(一)、出現(xiàn)上面爆邊
(1) The top edge appears
1、主鋸片太鈍,鋸齒太少
1. The main saw blade is too blunt and the saw teeth are too few
2、主鋸片高出板材太少
2. The main saw blade is too little higher than the plate
3、板材質(zhì)量太差,會很快鈍鋸片
3. If the quality of the plate is too poor, the saw blade will be blunt soon
4、重新更換鋸片
4. Replace the saw blade again
5、升高主鋸片
5. Raise the main saw blade
6、選用雜質(zhì)少、質(zhì)量高的板材
6. Select the plate with less impurities and high quality
(二)、出現(xiàn)下面爆邊(鋸后的板材)
(2) There is edge burst below (sawn board)
1、副鋸片太鈍
1. The saw blade is too blunt
2、副鋸寬度不夠、太窄
2. The width of the auxiliary saw is not enough or too narrow
3、主、副鋸片中間線不重合
3. The middle line of the main saw blade and the auxiliary saw blade does not coincide
4、重新更換鋸片
4. Replace the saw blade again
5、換鋸片或增加鋸片厚度
5. Change saw blade or increase saw blade thickness
6、重新調(diào)整副鋸左右位置
6. Readjust the left and right position of the auxiliary saw
(三)、有燒焦的痕跡(鋸后板材上)
(3) There are burning marks (on the sawn plate)
1、合金鋸片太鈍,鋸片上鋸齒太多
1. The alloy saw blade is too blunt and there are too many teeth on the saw blade
2、轉(zhuǎn)速過高或進(jìn)料太慢
2. Too high speed or too slow feeding
3、更換鋸片,選擇適當(dāng)?shù)匿徠?/div>
3. Replace the saw blade and select the appropriate one
4、選擇適當(dāng)?shù)霓D(zhuǎn)速和進(jìn)料速度
4. Select the appropriate speed and feeding speed
(四)、在鋸切時有工件被副鋸頂起來的現(xiàn)象
(4) During sawing, the workpiece is jacked up by the auxiliary saw
1、副鋸片太鈍
1. The saw blade is too blunt
2、副鋸片升得太高
2. The auxiliary saw blade rises too high
3、更換鋸片
3. Replace the saw blade
4、適當(dāng)降低副鋸片高度
4. Reduce the height of the auxiliary saw blade appropriately
(五)、中間貼面板爆邊
(5) Edge burst of middle panel
1、板材較厚,每塊微彎不平整,上下面互疊一起后產(chǎn)生縫隙
1. The plate is thick, each piece is slightly bent and uneven, and the upper and lower parts are overlapped to form a gap
2、機(jī)械壓料的氣缸壓力不夠
2. The cylinder pressure of mechanical pressing is not enough
3、工件板面有條紋(凹凸)也會爆邊
3. The work piece plate surface has the stripe (concave convex) also can burst the edge
4、工作鋸切時少壓2-3塊板材
4. Press 2-3 pieces less when sawing
5、鋸切板材時進(jìn)刀速度適當(dāng)調(diào)慢適切認(rèn)可
5. When sawing the plate, the feed speed should be adjusted to be appropriate
6、檢查鋸片是否不鋒利,及時修磨刃口
6. Check whether the saw blade is not sharp, and repair the edge in time
感謝您的閱讀,希望以上內(nèi)容對您有所幫助,如您想了解更多精彩內(nèi)容請點擊我們的官網(wǎng):富美家山東總代理http://。
Thank you for your reading. I hope the above content will be helpful to you. If you want to know more wonderful content, please click our official website: fumika Shandong general agent http:// .
分類導(dǎo)航
Related products相關(guān)新聞
- 富美家色麗石:色麗石臺面出現(xiàn)裂紋時,該如何修補(bǔ)?2024-11-16
- 你們知道富美家美耐板的優(yōu)缺點嗎?2024-10-18
- 富美家防火板怎么安裝施工2024-10-14
- 富美家美耐板:如何正確選購防火板?2024-09-04
- 美耐板和三胺板的區(qū)別2024-08-22
- 富美家防火板尺寸有哪些?2024-08-05
- 富美家防火板的應(yīng)用領(lǐng)域介紹2024-08-01
- 防火板等級標(biāo)準(zhǔn)分為B1級、B2級和B3級三個等級2024-07-08
- 富美家抗倍特板的材質(zhì)是什么?2024-06-24
- 富美家抗倍特隔斷的使用特點2024-06-19